Analysis of furniture wood grain decorative paper in the use of precautions

Category : Company NewsDate:2023-06-01

Furniture paper can change the shape of the furniture, in the process of Posting if there are wrinkles will affect the overall effect of furniture decoration, need to tear off and start again. If you want to avoid wrinkles before Posting should be prepared, under normal circumstances, used as a sticker substrate for particleboard density board, and if directly on the surface of these two plates stickers, there will often be uneven problems, so the substrate must be treated to make it smooth and smooth.

Furniture paper: Furniture paper, as the name suggests, is the use of wood grain paper veneer board as a furniture substrate. Wood grain paper veneer is different from solid wood and wood veneer, but it has the effect of wood grain. In general, painting sticker furniture should mainly pay attention to the following aspects:


First, the treatment of the substrate: under normal circumstances, the substrate used as a sticker is mostly particled-density board, and if the sticker is directly on the surface of the two plates, there will often be an uneven paste problem, so the substrate must be treated to make it smooth and smooth. Such as on the board full of a lot of water ash, scraping putty, spray PU or PE solid color primer and so on. The advantage of a full batch of water ash is low cost, and its disadvantage is mainly the problem of adhesion. Although the putty solves the adhesion problem with the substrate, we know that the putty on the market is mostly single-component nitrocellulose putty, and from the compatibility of the paint, it is easy to cause the reaction between the upper polyester thinner and the biting phenomenon. Spraying PU or PE solid color primer will not cause the above problems. Therefore, it is also the current Z as popular.

Second, the selection of paint: the effect of sticker furniture is good or bad, the first thing is to look at its transparency, followed by color, fullness, hardness, feel and so on. If the transparency of the paint is not good, it will directly affect the clarity and perception of the color. Therefore, it is important to choose a good transparent paint. For example, we can choose CR PU PD3900, PD3300, PD3600, and PD1500 transparent primers and PE ED3100, ED3300, ED3600 and ED3900 transparent primers, etc., while achieving high transparency, It also has good filling force, fullness, hardness, yellowing resistance, grinding and other different effects. Top paint, we can choose PU P3600X, P3800X, P3400X and P2800X and PE ED3000, which not only ensures good transparency, but also meets the requirements of film hardness, scratch resistance, fullness, feel, yellow resistance and so on.

Third, coating process: the quality of furniture is good or bad, the effect is not only dependent on the quality of the plate. The quality of the paint, and the choice of a reasonable coating process is also very important. In general, the process of painting sticker furniture can be divided according to the following processes:


1, white processing. Use 240# - 320# sandpaper to remove surface stains and make the surface smooth.

2. Closure. Seal it with CR PS900 bottom Depot and polish it after 3-4 hours.

3. Polish. Gently grind with 320# sandpaper to remove wood bristles and spines.

4. Primer. Spray CR PU or PE solid color primer to achieve a certain fullness and hiding power, no leakage bottom, 5-8 hours after polishing.

5. Polish. Sand thoroughly with 320# sandpaper, smooth and flat.

6. Stickers. With wood grain paper, the stickers are required to be no bubbles, no wrinkles, neat and consistent, and the primer is applied after 24 hours of hard work.

7. Primer. Spray CR PU or PE transparent primer, reach a certain fullness, 5-8 hours after polishing.

8. Polish. Smooth and smooth with 400# -600 # grinding, requiring no obvious sand marks, no bright spots.

9. Touch up the color. Mix CR SRNA or color essence and clear paint according to proportion, spray, require uniform color, 8-10 hours of hard work after grinding.

10. Polish. Lightly grind with 800# - 1000# sandpaper to remove surface particles.

11. Cover the light. With China Resources clear paint, spray, require filtration, pay attention to dust, 24 hours after work.


The effect of furniture paper is always good or bad quality, transparency, color, fullness, hardness, feel and so on all affect its frying, with a good material after the corresponding process will have a different effect. The quality of furniture is good or bad, and the effect is not only dependent on the quality of the plate. The quality of the paint, and the choice of a reasonable coating process is also very important.